DAMAGE ASSESSMENT FOR BRICK BUILDINGS WITH CLAY TILE ROOFING
This section provides a damage assessment by visual screening of damaged brick buildings with clay tile roofing and provides links to the measures required for rehabilitation of such buildings.

DAMAGE CATEGORY G-1
DAMAGES OBSERVED
-
Thin cracks in plaster
-
Falling of plaster in bits and pieces in limited parts
ACTION REQUIRED
-
Go to retrofitting

DAMAGE CATEGORY G-2
DAMAGES OBSERVED
-
Small cracks in walls through thickness
-
Falling of plaster in large bits over large areas
-
Damage to non-structural parts like projecting chajjas etc. where present in the buildings
-
Disturbance of roofing tiles
ACTION REQUIRED
-
Go to retrofitting

DAMAGE CATEGORY G-3
DAMAGES OBSERVED
-
Large and deep cracks in walls
-
Widespread cracking of walls including corners
-
Widespread displacement and falling of tiles
-
Separation and tilting of wall portions
ACTION REQUIRED
-
Go to retrofitting

DAMAGE CATEGORY G-4
DAMAGES OBSERVED
- Gaps occur in walls
- Some thick walls show delamination and falling of masonry on one face
- Some walls collapse partly or wholly
- Large separation of walls at the corners
- About 50% of the walls fail resulting in dangerous state of the building
- Parts of the roof may collapse
ACTION REQUIRED
-
Unsafe building- stay away
-
Evacuate immediately
-
Consult technical expert

DAMAGE CATEGORY G-5
DAMAGES OBSERVED
-
Complete collapse of the building
ACTION REQUIRED
- Unsafe building and stay away
- Archive building material for temporary shelter and avoid pilfering.